Proposed Modifications to ACI 318-95 Tension Development and Lap Splice Provisions for High-Strength Concrete

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Proposed Modifications to ACI 318-95 Tension Development and Lap Splice Provisions for High-Strength Concrete

Author(s): Azizinamini, A.; Darwin, D.; Eligehausen, R.; Pavel, R.; and Ghosh, S. K.

Publication: 318Reference

Volume: 12

Issue: 12

Appears on pages(s): pp. 922-926.

Keywords:

Date: 6/1/2011

Abstract:
ACI Structural Journal, V. 96, No. 6, Nov.-Dec. 1999