Title: Tests to Determine Performance of Deformed Welded Wire Fabric Stirrups

Author(s): Griezic, A.; Cook, W. D.; and Mitchell, D.

Publication: 318Reference

Volume: 11

Issue: 19

Appears on pages(s): pp. 211-220.

Keywords:

Date: 6/1/2011

Abstract:
ACI Structural Journal, V. 91, No. 2, Mar.-Apr. 1994