Title: Effect of Rust and Scale on the Bond Characteristics of Deformed Reinforcing Bars

Author(s): Kemp, E. L.; Brezny, F. S.; and Unterspan, J. A.

Publication: 318Reference

Volume: 7

Issue: 4

Appears on pages(s): pp. 743-756.

Keywords:

Date: 6/1/2011

Abstract:
ACI JOURNAL, Proceedings V. 65, No. 9, Sept. 1968