CONCRETE FOR INDUSTRIAL FLOORS

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: CONCRETE FOR INDUSTRIAL FLOORS

Author(s): Paul Horst Seiler

Publication: ANAPRE

Volume:

Issue:

Appears on pages(s):

Keywords: CONCRETE FOR INDUSTRIAL FLOORS

Date: 3/1/2009

Abstract:
In this article there are some important informations about concrete design for industrial floor such as aggregates, fibers and admixture.


ANAPRE, International Partner Access.

View Resource »