Title: Durability of masonry mortar

Author(s): Cement Concrete & Aggregates Australia

Publication: CCAA

Volume:

Issue:

Appears on pages(s): 7 pages

Keywords: durability, masonry mortar, composition, joint finish, marine exposure

Date: 3/1/2007

Abstract:
This Technical note presents the outcome of a major research project conducted by CCAA to investigate factors affecting the durability of masonry mortar. It examines the influence of masonry unit, mortar type and composition and joint finish on the potential durability of mortar in marine exposure.