Title: Joint Repair With MMA-Polymer Concrete

Author(s): Pete Barlow and Chris Olson

Publication: Concrete International

Volume: 12

Issue: 9

Appears on pages(s): 59-60

Keywords: airports; aprons; concrete pavements; cracking (fracturing); drying shrinkage; joint fillers; polymerization; polymethyl methacrylate; polymer-portland cement concrete; repairs; spalling; General

Date: 9/1/1990

Abstract:
Describes the evaluation of an unsatisfactory repair of spalled joints in an airport apron with methacrylate polymer concrete, the remedial action taken, and proper materials handling and application techniques to achieve a durable repair with this material.