Shear Strength of High-Strength Concrete Beams with Web Reinforcement

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Shear Strength of High-Strength Concrete Beams with Web Reinforcement

Author(s): Roller, J. J., and Russell, H. G.

Publication: 318Reference

Volume: 11

Issue: 9

Appears on pages(s): pp. 191-198

Keywords:

Date: 6/1/2005

Abstract:
ACI Structural Journal, V. 87, No. 2, Mar.-Apr. 1990


Free Access

View Resource »