Title: Comparative Study of Prestressed Concrete Beams, with and without Bond

Author(s): Mattock, A. H.; Yamazaki, J.; and Kattula, B. T.

Publication: 318Reference

Volume: 18

Issue: 8

Appears on pages(s): pp. 116-125

Keywords:

Date: 6/1/2005

Abstract: