Influence of Ties on the Behavior of Reinforced Concrete Columns

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Influence of Ties on the Behavior of Reinforced Concrete Columns

Author(s): Pfister, J. F.

Publication: 318Reference

Volume: 7

Issue: 15

Appears on pages(s): pp. 521-537

Keywords:

Date: 6/1/2005

Abstract:
ACI JOURNAL, Proceedings V. 61, No. 5, May 1964