In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Chat with Us Online Now
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: 523.1R-06: Guide for Cast-in-Place Low-Density Cellular Concrete
Author(s): ACI Committee 523
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 13
Keywords: cellular concrete; engineered fill; foaming agent; geotechnical fill; insulating concrete; insulating concrete roof decks; low-density cellular concrete; low- density controlled low-strength material (LD-CLSM); preformed foam.
Date: 8/15/2006
Abstract:This guide provides information on the materials, properties, design, proper handling, and applications of cast-in-place low-density cellular concretes having oven-dry densities of 50 lb/ft3 (800 kg/m3) or less. Roof deck systems and geotechnical applications often incorporate these lowdensity cellular concretes.