Title: Payment Provisions for Shotcrete as Seen by the Owner

Author(s): Frank L. Lynch

Publication: Special Publication

Volume: 54

Issue:

Appears on pages(s): 273-276

Keywords:

Date: 1/1/1977

Abstract:
The Washington Metropolitan Area Transit Authority (WMATA) officially came into existence in February 1967 after the District of Columbia, Maryland, and Virginia joined in a compact pursuant to Federal creative legislation signed the previous November to build a regional rapid rail transit system called METRO (1, 2).