Title: Torsional Stiffness of Reinforced Cocnrete Bridge Girders

Author(s): G.S. Pandit

Publication: Symposium Paper

Volume: 26

Issue:

Appears on pages(s): 634-662

Keywords: beams (supports); bending; bridges (structures); girder bridges; girders; reinforced concrete; research; shear properties; stiffness; structural analysis; torsion

Date: 1/1/1971

Abstract:
Torque-twist characteristics of reinforced concrete beams subjected to pure torsion, combined bending and torsion as well as combined bending, torsion and shear have been considered. . .A fair agreement between the computed and observed angles of twist was obtained.




  