Strength of Polymer and Polymer-Fibrous Concretes

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Strength of Polymer and Polymer-Fibrous Concretes

Author(s): T.S. Nagaraj, K.T. Sundara Raja Iyengar, and C.S. Viswanatha

Publication: Special Publication

Volume: 58

Issue:

Appears on pages(s): 139-160

Keywords: coarse aggregates; compressive strength; fiber reinforced concretes; impregnating; metal fibers; polymer concrete; synthetic fibers

Date: 1/1/1978

Abstract:
With the continued research efforts, presently the techniques of production of polymer impregnated concretes have been fairly understood. Measured and evaluated mechanical properties and durability aspects of this material reveal that dramatic improvements are possbile thereby offering great potential to this material in building industry.