Title: Durability of Concrete and Concrete Structures by Slow Cycle Fatigue

Author(s): Arnold Wilson

Publication: Symposium Paper

Volume: 47

Issue:

Appears on pages(s): 259-292

Keywords: air entrainment; bond (paste to aggregate); compressive strength; concretes; cracking (fracturing); curing; cyclic loads; deterioration; durability; dynamic modulus of elasticity; dynamic tests; fatigue tests; freeze-thaw durability; modulus of elasticity

Date: 1/1/1975

Abstract:
The purpose of this research was to develop and evalute a slow cycle fatigue method of testing concrete which might relate in part ot the durability of concret subjected to cyclic loading conditions.




  