Title: Polymer Concrete - Reinforced Concrete Composite Beams

Author(s): James Lott, Dan Naus, and Paul Howdyshell

Publication: Special Publication

Volume: 40

Issue:

Appears on pages(s): 295-318

Keywords: beams (supports); composite construction (concrete to concrete); compressive strength; creep properties; fiber reinforced concretes; polyster resins; polymer concrete; portland cements; precast concrete; reinforced concrete; portland cements

Date: 1/1/1973

Abstract:
Composite beams consisting of reinforced concrete and a layer or cap of polyester concrete in the region of high compressive stress are tested and evaluated.