Bibliography on Vibrations of Concrete Structures

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Bibliography on Vibrations of Concrete Structures

Author(s): Edward G. Nawy and Gajanan M. Sabnis

Publication: Special Publication

Volume: 60

Issue:

Appears on pages(s): 285-296

Keywords: bibliographies; prestressed concrete; reinforced concrete; vibrations

Date: 1/1/1979

Abstract:
The references listed in the following pages cover a good selection of research papers and applications in the area of vibrations of structural elements and systems.