Title: Quality Concrete Production for the California State Water Project

Author(s): John H. Lawder and Robert F. Adams

Publication: Special Publication

Volume: 104

Issue:

Appears on pages(s): 261-274

Keywords: compressive strength; concretes; inspection; quality assurance; quality control; statistical analysis; tests; water supply; General

Date: 10/1/1987

Abstract:
The organization and procedures used in the quality production of about 8 million cubic yards of concrete of all kinds for the California Water Project are described. These included design aspects, specifications, the concrete laboratory, and construction