Title: Effect of Maximum Size Agregate on Compressive Strength of Mass Concrete

Author(s): Elmo C. Higginson, George B. Wallace, and Elwood L. Ore

Publication: Special Publication

Volume: 6

Issue:

Appears on pages(s): 219-256

Keywords:

Date: 1/1/1963

Abstract:
Results of an extensive series of tests to determine the influence of the maximum aggregate size on compressive strength are reported. A wide range of cement content and aggregate sizes were used in the large test specimens, used to minimize the effect of speciment size.