Title: Lateral Displacement Ductility of Reinforced Concrete Flat Plates

Author(s): Pan, A, and Moehle, J. P.

Publication: 318Reference

Volume: 21

Issue: 13

Appears on pages(s): pp. 250-258.

Keywords:

Date: 6/1/2008

Abstract:
ACI Structural Journal, V. 86, No. 3, May-June, 1989