Title: Design of Connections of Earthquake Resisting Precast Reinforced Concrete Perimeter Frames

Author(s): Restrepo, J.; Park, R.; and Buchanan, A.

Publication: 318Reference

Volume: 21

Issue: 40

Appears on pages(s): pp. 68-80.

Keywords:

Date: 6/1/2008

Abstract:
Precast/Prestressed Concrete Institute Journal, V. 40, No. 5, 1995