Title: Curing of Concrete

Author(s): Bryant Mather

Publication: Symposium Paper

Volume: 104

Issue:

Appears on pages(s): 145-160

Keywords: cold weather construction; concretes; curing; curing compounds; evaporation; hot weather construction; mass concrete; moist curing; moisture content; plastic shrinkage; reinforced concrete; reviews; temperature; Materials Research

Date: 10/1/1987

Abstract:
If concrete is to be permitted to demonstrate that the materials and proportions selected for its production were appropriate for its intended service, the construction practices used in making, placing, consolidating, and curing it must also be appropria




  