Title: New-Old Theory of Reinforced Concrete Beams in Bending

Author(s): L.J. Mensch

Publication: Journal Proceedings

Volume: 10

Issue: 12

Appears on pages(s): 28-41

Keywords: none

Date: 12/1/1914

Abstract:
Practically all ordinances of American and European building authorities insist on the following assumptions and requirements for the design of reinforced concrete slabs and beams . . .