Title: Design of Reinforced Concrete Footings for Buildings

Author(s): R.L. Bertin

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 389-393

Keywords: none

Date: 2/1/1916

Abstract:
The use of concrete, plain and reinforced, for the construction of foundation for all types of structures, has replaced almost exclusively all other materials, such as wood, brick or stone masonry and structural steel.