Title: Standard Recommended Practice for Portland Cement Stucco

Author(s): ACI Committee on Standard Recommended Practice for Portland Cement Stucco

Publication: Journal Proceedings

Volume: 16

Issue: 2

Appears on pages(s): 304-327

Keywords: none

Date: 2/1/1920

Abstract:
Whenever the design of the structure permits, an overhanging roof or similar projection is recommended to afford protection to the stucco.