Title: Concrete Products Plant Operation

Author(s): ACI Committee P-6

Publication: Journal Proceedings

Volume: 22

Issue: 2

Appears on pages(s): 673

Keywords: none

Date: 2/1/1926

Abstract:
Committee P-6 felt that it would be desirable to elaborate on the curing tests reported at the 1925 convention to cover curing conditions during the whole year. A sub-committee on curing was appointed which outlined a series of tests to determine the effect of weather conditions on the outdoor curing of concrete block.




  