Title: Reinforced-Concrete Bridges

Author(s): A.E. Lindau

Publication: Journal Proceedings

Volume: 20

Issue: 2

Appears on pages(s): 122-134

Keywords: none

Date: 2/1/1924

Abstract:
The new world opened to the architect and builder of buildings by the development of concrete and reinforced-concrete was likewise opened to the engineer and the builder of bridges.




  