Title: Proportioning Concrete Materials With Especial Reference to Highway Construction

Author(s): G.W. Hutchinson

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 148-176

Keywords: none

Date: 2/1/1925

Abstract:
Few data are available relating to the development of concrete, as a unit, for particular types of structures. From the indications of this paper, it appears logical and economic to depart from the universal application of single theory proportioning of concrete for all purposes. Greater economy may be secured by considering the type of structure when designing the concrete mixture.