Title: SP-185: High-Performance Fiber Reinforced Concrete in Infrastructural Repair and Retrofit

Author(s): Editors: Neven Krstulovic-Opara and Ziad Bayasi

Publication: Special Publication

Volume: 185

Issue:

Appears on pages(s): 251

Keywords:

Date: 2/1/2000

Abstract:
SP-185 Up until now there has been very little information on the use of high-performance fiber-reinforced concrete (HPFRC). But recent laboratory studies and field applications show that HPFRC improves performance of civil engineering infrastructure in a cost-effective manner. This publication includes 11 papers on the mechanical properties of HPFRC for infrastructural repair and retrofit.