Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-5 of 68 Abstracts search results
Document:
21-291
Date:
September 1, 2023
Author(s):
Hak-Young Kim, Keun-Hyeok Yang, and Hye-Jin Lee
Publication:
Materials Journal
Volume:
120
Issue:
5
Abstract:
The purpose of this study is to investigate the effect of steel fiber content and type on the compressive and flexural ductility capacities of lightweight aggregate concrete (LWAC). Fiber-reinforced LWAC specimens were divided into four groups according to the type of fibers, such as conventional macrosteel fibers (SFs) with hooked ends, straight copper-coated microsteel fibers (CMSFs), crimping-shaped CMSFs, and hooked-end CMSFs. The fibervolume fractions (Vf) were 0.5, 1.0, and 1.5%. This study also modifies the ASTM C1018 method by using the initial crack point calculated from the elastic theorem to save a tedious and elaborated effort in determining the reference point at the load-deflection curve, particularly for beams with a strong hardening response. The test results revealed that the hooked-end CMSFs were better than SFs and crimping-shaped CMSFs with the same shape and length at decreasing the slope of the applied loads at descending branches of the compressive stress-strain and flexural load deflection curves for the LWAC. Compressive and flexural toughness indexes were derived as functions of the fiber reinforcing index based on the regression analysis of test data to assess the ductility improvement of LWAC with steel fibers.
DOI:
10.14359/51737185
21-483
Nima Mohammadian Tabrizi, Davood Mostofinejad, and Mohammad Reza Eftekhar
This paper is aimed at investigating the effects of different fiber inclusion on the mechanical properties of ultra-high-performance concrete (UHPC) by adding mineral admixtures as cement replacement materials to reduce production costs and CO2 emissions of UHPC. Throughout this research, 21 mixture designs containing four cement substitution materials (silica fume, slag cement, limestone powder, and quartz powder) and three fibers (steel, synthetic macrofibers, and polypropylene) under wet and combined (autoclave, oven, and water) curing were developed. To investigate the mechanical properties in this research, a total of 336 specimens were cast to evaluate compressive strength, the modulus of rupture (MOR), and the toughness index. The findings revealed that at the combined curing, regarded as a new procedure, all levels of cement replacement recorded a compressive strength higher than 150 MPa (21.76 ksi). Furthermore, the mechanical properties of the mixture design containing microsilica and slag (up to 15%) were found to be higher than other cement substitutes. Also, it was shown that all levels of the fiber presented the MOR significantly close together, and samples made of synthetic macrofibers and steel fibers exhibited deflection-hardening behavior after cracking. The mixture design containing microsilica, slag, limestone powder, and quartzpowder, despite the significant replacement of cement (approximately 50%) by substitution materials, experienced a slight drop in strength. Therefore, the development of this mixture is optimal both economically and environmentally.
10.14359/51738888
21-392
November 1, 2022
Arjun Siva Rathan R. T., Sunitha V., and Anusudha V.
119
6
Interlocking concrete block pavement (ICBP) is one of the pavement types adopted worldwide. The influential parameter of ICBP is comparatively more, which includes the geometric parameters of the interlocking paver blocks such as the size, shape, thickness, strength, and laying pattern of the blocks, and the gradations of the jointing and bedding sand. Other than the wearing surface, the thickness and properties of the bedding sand, base, and subgrade also play a vital role in the deflection properties of ICBP. The objective of the present study is to analyze the influence of block thickness, base thickness, and granular layer thickness on the deflection behavior and stress distribution of ICBP. The block thicknesses used for this study are 80, 100, and 120 mm; the bedding sand thicknesses are 30, 50, and 70 mm; and the base thicknesses are 150, 300, and 450 mm. The experimental work is carried out using the laboratory plate load test to determine the deflection and stress distribution of ICBP. Numerical analysis is also employed to simulate laboratory testing. The study attempts to find the most influential factor and the optimized parametric value for attaining lower deflection using Design-Expert software. The test results conclude that the thicknesses of the block and granular layer play an imperative role among the considered parameters.
10.14359/51736002
21-077
September 1, 2022
Abbas Rezaeian, Amir Daghari, and Venkatesh Kodur
This paper presents the results of an experimental study on the comparative response of polypropylene (PP) fiber-incorporated reinforced concrete (RC) beams under fire conditions. Five fullscale RC beam specimens, made with different batch mixtures comprising normal plain concrete (NPC) and fiber-reinforced concrete (FRC), were tested to assess their spalling performance and structural behavior under fire conditions. The main variables in the experiments were the amount and length of PP fibers. Deflections, temperatures, and spalling in the beams were monitored during fire exposure. FRC beams’ flexural failure occurs after 151 minutes at heating temperatures beyond 850°C, when deflections exceed span/20. When the concrete contains PP fibers (that is, FRC beams), the gamut of fire-induced spalling in RC beams gets reduced, increasing the fire resistance from 147 to 171 minutes (approximately 17%). Furthermore, test results show that adding 2 to 3 kg/m3 of PP fibers effectively releases the pore pressure through tensile cracking and reduces the amount of spalling in the FRC beams.
10.14359/51735947
21-161
March 1, 2022
Alessandro P. Fantilli and Farmehr M. Dehkordi
2
Experimental research performed on fiber-reinforced cement-based composites made with polymeric aggregate and reinforced with recycled steel fibers is presented in this paper. In total, 18 concrete prisms were cast with a two-stage procedure: first, the fibers from end-of-life tires were put in the molds and, subsequently, they were covered by a cementitious grout containing fine (recycled or virgin) aggregate. The two-stage composites showed more than one crack and a deflection-hardening behavior in the post-cracking regime by performing three-point bending tests. Moreover, both flexural and compressive strength increased with the fiber volume fraction. Thus, if the content of recycled materials is suitably selected, the ecological and mechanical performances of the two-stage composites improve and become similar to those of one-stage fiber-reinforced concrete made with only virgin components.
10.14359/51734300