ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

Showing 1-5 of 1734 Abstracts search results

Document: 

SP361

Date: 

March 1, 2024

Author(s):

ACI Committees ACI Committees 130 and E702

Publication:

Symposium Papers

Volume:

361

Abstract:

Concrete has played a pivotal role in shaping the modern world’s infrastructure and the built environment. Its unparalleled versatility, durability, and structural integrity have made it indispensable in the construction industry. From skyscrapers to long-span bridges, water reservoirs, dams, and highways, the ubiquitous presence of concrete in modern society underscores its significance in global development. As we stand at the crossroads of environmental awareness and the imperative to advance our societies, the sustainability of concrete production and utilization is becoming a new engineering paradigm. The immense demand for concrete, driven by urbanization and infrastructure development, has prompted a critical examination of its environmental impact. One of the most pressing concerns is the substantial carbon footprint associated with traditional concrete production. The production of cement, a key ingredient in concrete, is a notably energy-intensive process that releases a significant amount of carbon dioxide (CO2) into the atmosphere. As concrete remains unparalleled in its ability to provide structural functionality, disaster resilience, and containment of hazardous materials, the demand for concrete production is increasing, while at the same time, the industry is facing the urgency to mitigate its ecological consequences. This special publication investigates the multi-faceted realm of concrete sustainability, exploring the interplay between its engineering properties, environmental implications, and novel solutions, striving to provide an innovative and holistic perspective. In recent years, the concrete industry has witnessed a surge of innovation and research aimed at revolutionizing its sustainability. An array of cutting-edge technologies and methodologies has emerged, each offering promise in mitigating the environmental footprint of concrete. Notably, the integration of supplementary cementitious materials, such as calcined clays and other industrial byproducts, has gained traction to reduce cement content while enhancing concrete performance. Mix design optimization, coupled with advanced admixtures, further elevates the potential for creating durable, strong, and eco-friendly concrete mixtures. Concrete practitioners will gain an advanced understanding of a wide variety of strategies that are readily implementable and oftentimes associated with economic savings and durability enhancement from reading these manuscripts. The incorporation of recycled materials, such as crushed concrete and reclaimed aggregates, not only reduces waste but also lessens the demand for virgin resources. Furthermore, the adoption of efficient production techniques, along with the exploration of carbon capture and utilization technologies, presents an optimistic path forward for the industry. This special publication aspires to contribute to the ongoing discourse on concrete sustainability, offering insights, perspectives, and actionable pathways toward a more environmentally conscious future.

DOI:

10.14359/51740669


Document: 

SP-360_50

Date: 

March 1, 2024

Author(s):

Haitham A. Ibrahim, Mohamed F. M. Fahmy, and Seyed Saman Khedmatgozar Dolati

Publication:

Symposium Papers

Volume:

360

Abstract:

This study numerically investigates the long-term effectiveness of using externally bonded fiber-reinforced polymer (FRP) plates as a strengthening technique for reinforced concrete (RC) beams. A two-dimensional finite element model (FEM) that can accurately predict the flexural behavior of FRP strengthened RC beams, is developed. Weathering exposure time of 0.0, 15.5, 35, and 75 years were considered. In total, 28 different concrete beams were modelled using the developed FEM. The results show that prolonged exposure to natural weathering can cause premature FRP debonding, even before reaching the yielding load. The ultimate load capacity, midspan deflection, and ductility of strengthened RC beams can be reduced by up to 38%, 62%, and 100%, respectively. In addition, the findings raised concerns about the applicability of the ACI 440.2R-17 provisions for calculating the design flexural strength of FRP strengthened RC beams with prolonged exposure to natural weathering. To ensure a safe design for strengthened beams with FRP debonding or concrete crushing failure modes, this paper recommends an additional reduction factor ranging from 0.8 to 0.9. Furthermore, periodic inspection using non-destructive testing and FRP anchorage system are highly recommended for both existing and new applications of FRP in structures.

DOI:

10.14359/51740662


Document: 

SP-360_20

Date: 

March 1, 2024

Author(s):

Emmanuel Ferrier, Laurent Michel, Andrea Armonico

Publication:

Symposium Papers

Volume:

360

Abstract:

This paper presents the crack monitoring of reinforced concrete beams strengthened with fiber reinforced polymer (FRP) sheets. Emphasis is placed on the development of a smart FRP bonded material that can measure the crack opening of a reinforced concrete beam strengthened by FRP. The reliability measured by a conventional digital image correlation (DIC) and by the proposed smart FRP is employed to assess the contribution of the FRP to control the crack. The monitoring process is based on a large set of experimental database consisting of 19 test beams. The effect of FRP to control the crack opening is studied depending on the steel ratio, FRP ratio and the level of damaged of RC beams when FRP is applied. The results were compared with the theoretical values of crack width and spacing predicted using the Eurocode 2 (EC2) formula, calibrated for non-strengthened RC elements. The corresponding results were compared in order to clarify the effect of external bonded FRP on the cracking behaviour of RC beams.

DOI:

10.14359/51740632


Document: 

SP-360_16

Date: 

March 1, 2024

Author(s):

Ahmed Khalil, Rami A. Hawileh, and Mousa Attom

Publication:

Symposium Papers

Volume:

360

Abstract:

This study explores technological advancements enabling the utilization of GFRP bars in concrete structures, particularly in coastal areas. However, GFRP bars often encounter reduced bend strength at specific bend locations, which may pose a challenge in their practical application. Various properties such as the strength of bent GFRP bars are crucial for quality assurance, yet existing testing methods stated in ASTM D7914M-21 and ACI 440.3R-15 have limitations when applied to different GFRP bent shapes. Furthermore, those methods require special precautions to ensure symmetry and avoid eccentricities in specimens. To address these challenges, CSA S807:19 introduced a simpler standardized testing procedure that involves embedding a single L-shaped GFRP stirrup in a concrete block. However, the specified large block size in CSA S807:19 Annex E may pose difficulties for both laboratory and on-site quality control tests. Therefore, CSA S807:19 Annex E (Clause 7.1.2b) permits the use of a customized block size, as long as it meets the bend strength of the FRP bars without causing concrete splitting. To date, very few prior research has explored the use of custom block sizes. Therefore, this study aims to thoroughly investigate the strength of bent FRP bars with custom block sizes and without block confinement. Such an investigation serves to highlight the user-friendliness and efficiency of the CSA S807:19 Annex E method. The study recommends two block sizes: 200x400x300 mm (7.87x15.75x11.81 in) for bars <16 mm (0.63 in) diameter and 200x200x300 mm (7.87x7.87x11.81 in) for bars <12 mm (0.39 in). Additionally, the study cautions against using confinement reinforcement, especially with smaller blocks, as it could interfere with the embedded bent FRP bar. Furthermore, the study suggests incorporating additional tail length to mitigate the debonding effects resulting from fixing the strain gauges to the bent portion of the embedded FRP bar. By exploring these modifications, the study seeks to enhance the effectiveness of the testing procedure and expand its practical application for both laboratory and on-site quality assurance. The findings hold implications for the reliable testing of GFRP bars' strength, advancing their use as reinforcement in concrete structures.

DOI:

10.14359/51740628


Document: 

SP-360_41

Date: 

March 1, 2024

Author(s):

Yasser M. Selmy, Amr E. Abdallah, and Ehab F. El-Salakawy

Publication:

Symposium Papers

Volume:

360

Abstract:

The seismic performance of reinforced concrete (RC) structures relies on their ability to dissipate earthquake-induced energy through hysteric behavior. Ductility, energy dissipation, and viscous damping are commonly used as performance indicators for steel-RC seismic force-resisting systems (SFRSs). However, while several previous studies have proposed energy-based indices to assess energy dissipation and damping of steel-RC SFRSs, there is a lack of research on fiber-reinforced polymer (FRP)-RC structures. This study examines the applicability of the existing energy dissipation and damping models developed for steel-RC columns to glass FRP (GFRP)-RC ones, where the relationships between energy indices and equivalent viscous damping versus displacement ductility were analyzed for GFRP-RC circular columns from the literature. In addition, prediction models were derived to estimate energy dissipation, viscous damping, and stiffness degradation of such types of columns. It was concluded that similar lower limit values for energy-based ductility parameters of steel-RC columns can be applied to GFRP-RC circular columns, whereas the minimum value and analytical models for the equivalent viscous damping ratio developed for steel-RC columns are not applicable. The derived models for energy indices, viscous damping, and stiffness degradation had an R2 factor of up to 0.99, 0.7, and 0.83, respectively. These findings contribute to the development of seismic design provisions for GFRP-RC structures, addressing the limitations in current codes and standards.

DOI:

10.14359/51740653


12345...>>