Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-1 of 1 Abstracts search results
Document:
SP265-06
Date:
October 1, 2009
Author(s):
L.M. Gil-Martín, E. Hernández-Montes, M.A. Aschheim, and S. Pantazopoulou
Publication:
Symposium Papers
Volume:
265
Abstract:
This paper provides a theoretical overview on the most influential theories for compression field models for shear and torsion. Special attention is given to the steel behavior because this is the point where the rotating-angle softened-truss model (RA-STM) and modified compression field theory (MCFT) depart. A new proposal for the steel model is presented. This proposal has the advantage of an embedded bar system, but it does not introduce additional complexity in the formulation. The steel model is based on tension stiffening behaviour. Several examples are presented, including a prestressed girder and a wall-type structure.
DOI:
10.14359/51663293