Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-1 of 1 Abstracts search results
Document:
SP290-05
Date:
September 14, 2012
Author(s):
Robert T. Bates, Erik Holck, Miles Dee, Michael King
Publication:
Symposium Papers
Volume:
290
Abstract:
Constructing large capacity, monolithically placed water storage tank slabs is a complex proposition. Previously, specifying low-shrinkage concrete mixes and monolithic placement of the slab within a specified time period was the prescribed method, yet shrinkage cracking still occurred. We felt more could be done to improve concrete placing and finishing, reducing shrinkage cracking and enhance durability. An investigation on the use of an Internally Cured Concrete mix on the floor and roof slabs of the Denver Water 10-Million Gallon [MG] (38-Million Liter [ML]) Lone Tree Tank No. 2 that Bates Engineering Inc. was designing was pursued. The tank floor and roof slab are each about 61,000 ft2 (5,700 m2) and would be monolithically placed. Laboratory trial batches performed determined plastic and hardened characteristics of the ICC as compared to traditionally proportioned mix designs. Tests performed in the laboratory included: compressive strength and drying shrinkage (ASTM C 157(1), modified 7-day saturation). An ICC mix was selected based on durability expectations. Results of the floor slab placement were successful and only two shrinkage cracks were observed, 7-day and 28-day compressive strength tests, workability and consistency surpassed expectations. As a result, it was decided to use ICC concrete on the remaining structural components.
DOI:
10.14359/51684174