Title: Repairs to International Control Dam-Niagara Falls

Author(s): N. P. Bada

Publication: Symposium Paper

Volume: 93

Issue:

Appears on pages(s): 609-636

Keywords: bond (concrete to concrete); compressive strength; concrete construction; concrete dams; epoxy resins; mix proportioning; plasticizers; repairs; scarifying

DOI: 10.14359/6321

Date: 9/1/1986

Abstract:
Several of the bridge non air-entrained concrete bearing seats on the International Control Dam have concrete deterioration from the application of de-icing salts. A 410 tonne beam and deck slab assembly was raised by twelve hydraulic lift climbing jacks assembled to a single span Bailey Bridge Structure. The concrete repair consisted of removing the deteriorated concrete, application of an epoxy bonder, wood forming, and placing of good quality concrete. The 410 tonne beam and deck slab was lowered onto new elastomeric bearing pads to its original location. The paper details the construction procedures and methods of repair to concrete in Spans 2 and 4.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer