Title: Comparison of Known and Determined Water-Cement Ratios Using Petrography

Author(s): J. J. Liu and M. S. Khan

Publication: Symposium Paper

Volume: 191

Issue:

Appears on pages(s): 11-26

Keywords: alkali-silica reaction; concretes; deterioration; freezing and thawing; microscopy; petrography; porosity; water-cement ratio

DOI: 10.14359/5731

Date: 12/1/1999

Abstract:
At present, there are no standardized test methods for the determination of water-cement ratio (w/c) of a specimen of hardened concrete. Various methods that have been used include absorption of a water drop on a concrete surface, resistance of cement paste to scratching, polarized-light microscopy, and optical fluorescence microscopy. In these determinations, usually experience and judgment are heavily relied upon. In the absence of a reliable standardized technique, it is prudent to estimate the w/c by using specimens with known w/c and a combination of several techniques, rather than relying on a single technique. The objective of this paper is to demonstrate the successes achieved by following this approach. Concrete specimens with w/c of 0.30, 0.35, 0.40, 0.45, 0.50, 0.55, 0.60, 0.65, 0.70 were prepared and analyzed by visual examination, resistance to needle scratching, water absorption, and blue-dyed thin section techniques. This combined technique approach was then used to analyze concrete specimens from the field.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer