Impact Damage Retrofit of RC Bridge Girder Previously Retrofitted with CFRP Fabric

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Impact Damage Retrofit of RC Bridge Girder Previously Retrofitted with CFRP Fabric

Author(s): Abheetha Peiris and Issam Harik

Publication: Symposium Paper

Volume: 346

Issue:

Appears on pages(s): 31-50

Keywords: bridge; CFRP; heavy fabric; impact damage; reinforced concrete; retrofit SP-346: Field Applications of Non-Conventional Reinforcing and Strengthening Methods for Bridges and Structures 31

DOI: 10.14359/51730492

Date: 1/1/2021

Abstract:
Following an over-height truck impact, Carbon Fiber Reinforced Polymer (CFRP) fabric was used to retrofit the exterior girder in a four-span Reinforced Concrete Deck on Girder (RCDG) Bridge on route KY 562 that passes over Interstate 71 in Gallatin County, Kentucky. The impacted span (Span 3) traverses the two northbound lanes of Interstate 71. While the initial retrofit was completed in May 2015, a second impact in September 2018 damaged all four girders in Span 3. The previously retrofitted exterior girder (Girder 4) suffered the brunt of the impact, with all steel rebars in the bottom layer being severed. Damage to Girders 1, 2, and 3 was minor and none of the bars were damaged. A two-stage approach for the containment and repair of the damaged girders following an over-height truck impact was implemented when retrofitting the bridge. The repair and strengthening of all the girders using CFRP fabric was the economical option compared to the alternative option of replacing the RCDG bridge. The initial CFRP retrofit was found to have failed in local debonding around the impact location. The CFRP retrofit material that was not immediately near the impact location was found to be well bonded to the concrete. The removal of this material and subsequent surface preparation for the new retrofit was time consuming and challenging due to traffic constraints. In Girder 4 all but one of the main rebars were replaced by removing the damaged sections and installing straight rebars connected to the existing rebars with couplers. One of the rebars could not be replaced. A heavy CFRP unidirectional fabric, having a capacity of 534 kN (120,000 lbs.) per 305 mm (1 ft.) width of fabric, was selected for the flexural strengthening and deployed to replace the loss in load carrying capacity. A lighter unidirectional CFRP fabric was selected for anchoring and shear strengthening of all the girders, and to serve as containment of crushed concrete in the event of future over-height impacts. The retrofit with spliced steel rebars and CFRP fabric proved to be an economical alternative to bridge replacement.

Related References:

1. ACI Committee 440, 2008, Guide to the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures, ACI 440.2R-08, American Concrete Institute, Farmington Hills, MI.

2. AASHTO, 2012, Design of Bonded FRP Systems for Repair and Strengthening of Concrete Bridge Elements, 1st Edition, American Association of State Highway and Transportation Officials, Washington, D.C.

3. Schiebel, S., Parretti, R. and Nanni, A., 2001, “Repair and Strengthening of Impacted PC Girders on Bridge A4845 Jackson County, Missouri” Report No. RDT01-017, Missouri Department of Transportation, Jackson City, MO.

4. Wipf, T.J., Klaiber, F.W., Rhodes, J.D. and Kempers, B.J. 2004, “Effective Structural Concrete Repair –Volume 1 of 3: Repair of Impact Damaged Prestressed Concrete Beams with CFRP,” Iowa DOT Project TR-428, Iowa Department of Transportation, Ames, IA.

5. Nanni A., 2004, “Strengthening of an Impact-Damaged PC Girder,” Concrete Repair Bulletin, May/June, pp 16-20.

6. Harik, I. and Peiris, A., 2014, “Repair of Impacted Concrete Bridge Beams,” Proceedings of the 37th Symposium of the International Association for Bridge and Structural Engineering (IABSE-14), September 03-05, 2014, Madrid, Spain. 6 pages.

7. Tumialan, J.G., Huang, P.C., and Nanni, A. 2001. “Strengthening of an impacted PC girder on bridge A10062,” Final Report RDT01-013/RI99-041, Missouri Department of Transportation, Jackson City, MO.

8. Peiris, A., and Harik, I.E., 2017, “CFRP Rod Panels for Strengthening Concrete Bridges,” Advances in Structural Engineering Journal, Vol. 21(4), pp. 557-570.

9. Peiris, A., and Harik, I.E. 2018. “Design and Construction of CFRP Rod Panel Retrofit for Impacted RC Bridge Girders,” J. Compos. Sci., Vol. 2(3), 40.

10. Peiris, A., and Harik, I.E. 2019. “Improving the Durability of Impact Damaged PC Bridge Girders Using CFRP Rod Panel Retrofit,” ACI Special Publication, Vol. 331, pp. 80-100.

11. Harries, K. A., and Miller, R. 2012. “Updated Research for Collision Damage and Repair of Prestressed Concrete Beams," NCHRP 20-07/Task 307, National Cooperative Highway Research Program, Transportation Research Board, Washington, D.C.

12. Frankhauser, Jr., W., Elkaissi, J., Kahl, S., McMillan, S., Potter, W., Rister, D., Wilson, D., and O’Connor, J. 2015. “Advances in Fiber-Reinforced Polymer (FRP) Composites in Transportation Infrastructure,” NCHRP Project 20-68A, Scan 13-03, National Cooperative Highway Research Program, Transportation Research Board, Washington, D.C.

13. ICRI Committee 310, 2008, Guide for Surface Preparation for the Repair of Deteriorated Concrete Resulting from Reinforcing Steel Corrosion, ICRI 310.1R-2008 formerly No. 03730., International Concrete Repair Institute, St. Paul, MN.

14. ACI Committee 546, 2004, Concrete Repair Guide, ACI 564R-04, American Concrete Institute, Farmington Hills, MI.

15. Mirmiran, A., Shahawy, M., Nanni, A., Karbhari, V., Yalim, B. and Kalayci, A. 2008. “Recommended Construction Specifications and Process Control Manual for Repair and Retrofit of Concrete Structures Using Bonded FRP Composites," NCHRP Report 609, National Cooperative Highway Research Program, Transportation Research

Board, Washington, D.C.

16. Rosenboom, O., and Rizkalla, S.H., 2008. “Experimental Study of Intermediate Crack Debonding in Fiber-Reinforced Polymer Strengthened Beams,” ACI Structural Journal, Vol. 105(1), pp. 41-50.

17. Bonacci, J.F., and Maalej, M., 2000. “Externally Bonded Fiber-Reinforced Polymer for Rehabilitation of Corrosion Damaged Concrete Beams,” ACI Structural Journal, Vol. 97(5), pp. 703-711.

18. Ford, J.S., Chang, D.C., and Breen, J.E., 1981, “Behavior of Concrete Columns under Controlled Lateral Deformation,” ACI Journal, Jan.-Feb., pp. 3-20.

19. ICRI Committee 310, 2013, Selecting and Specifying Concrete Surface Preparation for Sealers, Coatings, Polymer Overlays, and Concrete Repair, ICRI 310.2R-2013, International Concrete Repair Institute, St. Paul, MN.