Title: ACI 506.2M-13(18) Specification for Shotcrete (SI Units)

Author(s): ACI Committee 506

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords: dry-mixture shotcrete; fiber-reinforced shotcrete; nozzleman; qualification; quality control; quality assurance; shooting; wet-mixture shotcrete

DOI:

Date: 11/12/2019

Abstract:
This specification contains the construction requirements for the application of shotcrete. Both wet- and dry-mixture shotcrete are addressed, as well as fiber-reinforced shotcrete. The minimum standard for materials, properties, testing, and application are covered. The materials, processes, quality control measures, and inspections described in this specification should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI certifications or equivalent.