Seismic Experiments and Analysis of Repaired Bridge Columns Using CFRP Donut

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Experiments and Analysis of Repaired Bridge Columns Using CFRP Donut

Author(s): Ruo-Yang Wu and Chris P. Pantelides

Publication: Symposium Paper

Volume: 333

Issue:

Appears on pages(s): 80-95

Keywords: analytical model; bond slip; damage; experiments, fiber reinforced polymer composites; low-cycle fatigue; plastic hinge relocation; repair; seismic

DOI: 10.14359/51720271

Date: 10/1/2019

Abstract:
Two severely damaged concrete column-to-cap beam specimens were successfully repaired, using a carbon fiber-reinforced polymer (CFRP) cylindrical shell, non-shrink repair concrete, and headed steel bars. The first cast-in-place specimen experienced concrete crushing and longitudinal bars fracture/buckling; for the second precast specimen, the column was completely separated from the cap beam. In this paper, two analytical models, Model Fiber and Model Rotational Spring (RS), simulating the seismic performance of the repaired specimens are proposed. In Model Fiber, plasticity considering bond-slip effects was distributed over the defined plastic hinge length of the nonlinear beam-column element. In Model RS, a non-linear rotational spring was used to consider the concentrated plasticity located at the repaired cross-section. Low-cycle fatigue of the damaged column longitudinal steel bars was included in the analytical models. Simulations show that the analytical results, in terms of hysteretic response and moment-rotation, are in very good agreement with the experimental results. Model fiber performed better for predicting the pinching effect in the hysteretic response of the repaired cast-in-place specimen; Model RS performed better for matching the hysteresis curves of the repaired precast concrete specimen. In addition, Model Fiber was able to predict the local response of the columns including the fracture of longitudinal bars due to low-cycle fatigue.

Related References:

1. M. J. N. Priestley, F. Seible, Y. Xiao, and R. Verma, “Steel jacket retrofitting of reinforced concrete bridge columns for enhanced shear strength-Part 1: Theoretical considerations and test design,” ACI Struct. J., vol. 91, no. 4, pp. 394–405, 1994.

2. F. Seible, M. J. N. Priestley, G. A. Hegemier, and D. Innamorato, “Seismic Retrofit of RC Columns with Continuous Carbon Fiber Jackets,” J. Compos. Constr., vol. 1, no. 2, pp. 52–62, 1997.

3. J. Gergely, C. P. Pantelides, and L. D. Reaveley, “Shear Strengthening RCT-joints Using CFRP Composites,” J. Compos. Constr., vol. 4, no. 2, pp. 56–64, 2000.

4. C. P. Pantelides, J. B. Duffin, and L. D. Reaveley, “Seismic Strengthening of Reinforced-Concrete Multicolumn Bridge Piers,” Earthq. Spectra, vol. 23, no. 3, pp. 635–664, 2007.

5. J. E. Parks, D. N. Brown, M. J. Ameli, and C. P. Pantelides, “Seismic repair of severely damaged precast reinforced concrete bridge columns connected with grouted splice sleeves,” ACI Struct. J., vol. 113, no. 3, pp. 615–626, 2016.

6. R.-Y. Wu and C. P. Pantelides, “Rapid seismic repair of severely damaged cast-in-place reinforced concrete bridge piers (No. 17-06278),” 2017.

7. R.-Y. Wu and C. P. Pantelides, “Rapid Seismic Repair of Severely Damaged Reinforced Concrete Bridge Piers,” in Structures Congress 2017, 2017, pp. 370–381.

8. R.-Y. Wu and C. P. Pantelides, “Rapid Repair and Replacement of Earthquake-damaged Concrete Columns Using Plastic Hinge Relocation,” Compos. Struct., vol. 180, pp. 467–483, 2017.

9. R.-Y. Wu and C. P. Pantelides, “Rapid Seismic Repair of Reinforced Concrete Bridge Columns,” ACI Struct. J., vol. 114, no. 5, pp. 1339–1350, 2017.

10. AASHTO, AASHTO guide specifications for LRFD seismic bridge design, 2nd ed. Washington D.C.: American Association of State Highway and Transportation Officials, 2011.

11. M. J. Ameli, J. E. Parks, D. N. Brown, and C. P. Pantelides, “Seismic evaluation of grouted splice sleeve connections for reinforced precast concrete column–to–cap beam joints in accelerated bridge construction,” PCI J., vol. 60, no. 2, pp. 80–103, 2015.

12. T. B. Panagiotakos and M. N. Fardis, “Deformation of reinforced concrete members at yielding and ultimate,” ACI Struct. J., vol. 98, no. 2, pp. 135–148, 2001.

13. R. Eligehausen, E. P. Popov, and V. V. Bertero, “Local Bond Stress-Slip Relationships of Deformed Bars under Generalized Excitations,” Proc. 7th Eur. Conf. Earthq. Eng., pp. 69–80, 1982.

14. J. Zhao and S. Sritharan, “Modeling of Strain Penetration Effects in Fiber-Based Analysis of Reinforced Concrete StructuresConcrete Structures,” ACI Struct. J., vol. 104, no. 2, pp. 133–141, 2007.

15. S. Mazzoni, F. McKenna, M. H. Scott, and G. L. Fenves, OpenSees Command Language Manual. Berkely, California: Pacific Earthquake Engineering Research Center, 2007.

16. F. Braga, R. Gigliotti, M. Laterza, M. D. Amato, and S. Kunnath, “Modified Steel Bar Model Incorporating Bond-Slip for Seismic Assessment of Concrete Structures,” J. Struct. Eng., vol. 138, no. November, pp. 1342–1350, 2012.

17. CEB-FIP, CEB-FIP Model Code 1990. Thomas Telford Ltd., London, 1993.

18. A. Vosooghi and M. S. Saiidi, “Design guidelines for rapid repair of earthquake-damaged circular RC bridge columns using CFRP,” J. Bridg. Eng., vol. 18, no. 9, pp. 827–836, 2013.

19. M. H. Scott and G. L. Fenves, “Plastic Hinge Integration Methods for Force-Based Beam–Column Elements,” J. Struct. Eng., vol. 132, no. 2, pp. 244–252, 2006.

20. P. Uriz, “Towards Earthquake Resistant Design of Concentrically Braced Steel Structures,” University of California, Berkeley, 2005.

21. R.-Y. Wu and C. P. Pantelides, “Concentrated and Distributed Plasticity Models for Seismic Repair of Damaged RC Bridge Columns,” J. Compos. Constr., vol. 22, no. 5, p. 04018044, 2018.

22. M. J. Ameli and C. P. Pantelides, “Seismic analysis of precast concrete bridge columns connected with grouted splice sleeve connectors,” J. Struct. Eng., vol. 143, no. 2, p. 04016176:1-13, 2016.

23. C. B. Haselton, A. B. Liel, S. C. Taylor-Lange, and G. G. Deierlein, “Calibration of Model to Simulate Response of Reinforced Concrete Beam-Columns to Collapse,” ACI Struct. J., vol. 113, no. 6, pp. 1141–1152, 2016.

24. L. F. Ibarra and H. Krawinkler, “Global Collapse of Frame Structures under Seismic Excitations,” Berkeley, California, 2005.