On the Application of Basalt-Fiber Reinforced Polymer (BFRP) Bars to Prestressed Slab Elements Typical of the Precast Concrete Industry

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: On the Application of Basalt-Fiber Reinforced Polymer (BFRP) Bars to Prestressed Slab Elements Typical of the Precast Concrete Industry

Author(s): Bruno Dal Lago, Davide Bisi and Liberato Ferrara

Publication: Symposium Paper

Volume: 333

Issue:

Appears on pages(s): 40-59

Keywords: basalt; creep; losses; nonlinear analysis; prestressing; serviceability; slab elements; structural design

DOI: 10.14359/51720269

Date: 10/1/2019

Abstract:
Basalt-Fiber Reinforced Polymer (BFRP) bars have been recently proposed to be used to prestress precast concrete elements. Mechanical properties, potential low production cost, low carbon footprint, and enhanced durability make the application of BFRP to prestressed concrete promising. Nevertheless, some issues related to anchorage and sustained stress still need to be fully addressed. Applications are so far limited to few laboratory tests. This paper discusses how the Serviceability Limit State (SLS) and Ultimate Limit State (ULS) checks of prestressed elements employing this technology vary with respect to elements pre-stressed with steel tendons. Furthermore, an attempt is made to investigate the potential application into the precast concrete industry, by analyzing several typical roof and floor slab elements with different cross-sections. This investigation highlights which type of element could be more advantageously switched to the use of pre-stressed BFRP bars, and at which cost in terms of structural performance.

Related References:

1. Nanni, A., Tanigaki, M., 1992, “Pretensioned prestressed concrete members with bonded fiber reinforced plastic tendons: development and flexural bond lengths (static)”, ACI Structural Journal, V.89, No.4, pp. 433-441.

2. Lees, J.M., Burgoyne, C.J., 1999, “Experimental Study of Influence of Bond on Flexural Behavior of Concrete Beams Pretensioned with Aramid Fiber Reinforced Plastics”, ACI Structural Journal, V.96, No.3, pp. 377-385.

3. Naaman, A.E., Tan, K. H., Jeong, S.M., Alkhairi, F.M., 1993, “Partially prestressed beams with carbon fiber composite strands: preliminary tests evaluation”, SP-138, ACI, pp. 441-464.

4. Stoll, F., Saliba, J.E., Casper, L.E., 2000, “Experimental study of CFRP-prestressed high-strength concrete bridge beams”, Composite Structures, V.49, pp. 191-200.

5. Taerwe, L.R., Lambotte, H., Miesseler, H.J., 1992, “Loading tests on concrete beams prestressed with glass fiber tendons”, PCI Journal, July-August, pp. 84-97.

6. Fiore, V., Scalici, T., Di Bella, G., Valenza, A., 2015, “A review on basalt fibres and its composites”, Composites Part B: Engineering, V.74, pp. 74-94.

7. High, C., Seliem, H.M., El-Safty, A., Rizkalla, S.H., 2015, “Use of basalt fibers for concrete structures”, Construction and Building Materials, V.96, pp. 37-46.

8. Taylor, S.E., Robinson, D., Sonebi, M., 2011, “Basalt-fibre-reinforced polymer reinforcement”, Concrete, April, pp. 48-50.

9. Tharmarajah, G., Taylor, S.E., Robinson, D., Cleland, D.J., 2015, “Corrosion resistant fibre reinforced polymer (FRP) reinforcement for bridge deck slabs”, Proceedings of the Institution of Civil Engineers: Bridge Engineering, V.168, No.3, pp. 208-217.

10. Zhang, L., Sun, Y., Xiong, W., 2016, “Experimental study on the flexural deflections of concrete beam reinforced with basalt FRP bars”, Materials and Structures, V.48, pp. 3279-3293.

11. Elgabbas, F., Vincent, P., Ahmed, E.A., Benmokrane, B., 2016, “Experimental testing of basalt-fiber-reinforced polymer bars in concrete beams”, Composites Part B: Engineering, V.91, pp. 205-218.

12. Fan, X., Zhang, M., 2016, “Experimental study on flexural behaviour of inorganic polymer concrete beams reinforced with basalt rebar”, Composites Part B: Engineering, V.93, pp. 174-183.

13. Fan, X., Zhang, M., 2016, “Behaviour of inorganic polymer concrete columns reinforced with basalt FRP bars under eccentric compression: An experimental study”, Composites Part B: Engineering, V.104, pp. 44-56.

14. Deegan, P., Taylor, S.E., Sonebi, M., Ferrara, L., Dal Lago, B., Pattarini, A., 2017, “An experimental study towards steel-free precast concrete elements”, Concrete, V. 51, No. 6, pp. 38-41.

15. Dal Lago, B., Ferrara, L., Taylor, S.E., Sonebi, M., Deegan, P., Kelly, G., Pattarini, A., 2017, “Full-scale testing and numerical analysis of a precast fibre reinforced self-compacting concrete slab pre-stressed with basalt fibre polymer bars”, Composites Part B: Engineering, V.128, pp. 120-133.

16. Atutis, E., Valivonis, J., Atutis, E., 2017, “Experimental study of concrete beams prestressed with basalt fiber reinforced polymers under cyclic load”, Composite Structures, V.183, pp.389-396.

17. Atutis, M., Valivonis, J., Atutis, E., 2017, “Experimental study of concrete beams prestressed with basalt fiber reinforced polymers. Part I: flexural behavior and serviceability”, Composite Structures, V. 183, pp. 114-123.

18. Atutis, M., Valivonis, J., Atutis, E., 2018, “Experimental study of concrete beams prestressed with basalt fiber reinforced polymers. Part II: stress relaxation phenomenon”, Composite Structures, V. 202, pp. 344-354.

19. Dal Lago, B., Dibenedetto, C., Palermo, A., Pampanin, S., Giorgini, S., Buchanan, A.H., Carradine, D., 2017, “Structural behavior of longitudinally post-tensioned timber beams under serviceability gravity loading”, Journal of Structural Engineering, ASCE, V. 143, No. 8, Paper No. 04017071.

20. McConnell, E., McPolin, D., Taylor, S.E., 2015, “Post-tensioning glulam timber beams with basalt FRP tendons. Proceedings of the Institution of Civil Engineers: Construction Materials, V.168, No.5, pp. 232-240.

21. ACI Committee 440.1R, 2015, Guide for the design and construction of structural concrete reinforced with fiber-reinforced polymer (FRP) bars (ACI 440.1R-15), American Concrete Institute, Farmington Hills, MI.

22. Giltrap, J.M., Burke, C.R., Dowden, D.M., Dolan, C.W., 1997, “Development of FRP reinforcement guidelines for prestressed concrete structures”, Journal of Composites in Construction, ASCE, V.1, No.4, pp. 131-139.

23. Dolan, C.W., Bakis, C.E., Nanni, A., 2001, Design recommendations for concrete structures pre-stressed with FRP tendons, Report of the FHWA No. DTFH61-96-C-00019.

24. Dolan, C.W., Swanson, D., 2002, “Development of flexural capacity of a FRP prestressed beam with vertically distributed tendons”, Composites Part B: Engineering, V.33, pp. 1-6.

25. Zou, P.X.W., 2003, “Flexural behaviour and deformability of fiber reinforced polymer prestressed concrete beams”, Construction and Building Materials, V.21, pp. 777-788.

26. Du, X., Zuohu, W., Jingbo, L., 2011, “Flexural capacity of concrete beams prestressed with carbon fiber reinforced polymer (CFRP) tendons”, Advanced Materials Research, VV.168-170, pp. 1353-1362.

27. Pisani, M.A., 2000, “Long-term behaviour of beams prestressed with aramid fibre cables: Part 1: a general method”, Engineering Structures, V.22, No.12, pp. 1641-1650.

28. Pisani, M.A., 2000, “Long-term behaviour of beams prestressed with aramid fibre cables: Part 2: an approximate solution”, Engineering Structures, V.22, No.12, pp. 1651-1660.

29. Bischoff, P.H., 2005, “Re-evaluation of deflection predictions for concrete beams reinforced with steel and FRP bars”, Journal of Structural Engineering, ASCE, V.131, No.5, pp. 752-767.

30. Youakim, S.A., Karbhari, V.M., 2007, “An approach to determine long-term behavior of concrete members prestressed with FRP tendons”, Construction and Building Materials, V.27, pp. 1052-1060.

31. Zou, P.X.W., Shang, S., 2007, “Time-dependent behaviour of concrete beams pretensioned by carbon fibrereinforced polymers (CFRP) tendons”, Journal of Composites for Construction, ASCE, V.7, No.4, pp. 275-284.

32. Knight, D., Visintin, P., Oehlers, D.J., 2016, “Displacement-based simulation of time-dependent behaviour of RC beams with prestressed FRP or steel tendons”, Structural Concrete, V.3, pp. 406-417.

33. Lou, T., Lopes, S.M.R., Lopes, A.V., 2016, “Time-dependent behavior of concrete beams prestressed with bonded AFRP tendons”, Composites Part B: Engineering, V.97, pp. 1-8.

34. Reda Taha, M., Shrive, N.G., 2003, “New concrete anchors for carbon fiber-reinforced polymer post-tensioning tendons - part 2: development/experimental investigation”, ACI Structural Journal, V.100, No.1, pp. 96-104.

35. Al-Mayah, A., Soudki, K., Plumtree, A., 2007, “Novel anchor system for CFRP rod: finite-element and mathematical models”, Journal of Composites for Construction, ASCE, September/October, pp. 469-476.

36. Carvelli, V., Fava, G., Pisani, M.A., 2009, “Anchor system for tension testing of large diameter GFRP bars”, Journal of Composites for Construction, ASCE, September/October, pp. 344-349.

37. Schmidt, J.W., Bennitz, A., Taljsten, B., Pedersen, H., 2010, “Development of mechanical anchor for CFRP tendons using integrated sleeve”, Journal of Composites for Construction, ASCE, July/August, pp. 397-405.

38. Wolff, R., 1987, “Heavy duty composite material for prestressing of concrete structures”, IABSE Paris-Versailles Symposium, IABSE Reports, V. 55, pp. 419-424.

39. Bellakehal, H., Zaidi, A., Masmoudi, R., Bouicha, M., 2014, “Behavior of FRP Bars-Reinforced Concrete Slabs under Temperature and Sustained Load Effects”, Polymers, V.6, No.3, pp. 873-889.

40. D’Antino, T., Pisani, M.A., Poggi, M., 2018, “Effect of the environment on the performance of GFRP reinforcing bars”, Composites Part B: Engineering, V.141, pp. 123-136.

41. D’Antino, T., Pisani, M.A., 2018, “Influence of sustained stress on the durability of glass FRP reinforcing bars”, Construction and Building Materials, V.187, pp. 474-486.

42. Dal Lago, B., 2017, “Experimental and numerical assessment of the service behaviour of an innovative longspan precast roof element”, International Journal of Concrete Structures and Materials, V.11, No. 2, pp. 261-273.

43. Dal Lago, B., Dal Lago, A., 2018, “New precast constructions for integrated complex urban interventions / Neue fertigteilkonstruktionen für integrierte komplexe städtische interventionen”, BFT International, V. 84, No. 4, pp. 72-80.

44. Garcia-Taengua, E., Sonebi, M., Crossett, P., Taylor, S.E., Deegan, P., Ferrara, L., Pattarini, A., 2016, “Performance of sustainable SCC mixes with mineral additions for use in precast concrete industry”, Journal of Cement Based Materials, V.5, No.3, pp. 157-175.

45. CEN-EN 14651:2005. Test method for metallic fibered concrete – Measuring the flexural tensile strength (limit of proportionality (LOP), residual). European Committee for Standardization, Brussels.

46. CEN-EN 1992-1-1:2005. Eurocode 2: Design of concrete structures. Part 1-1: general rules and rules for buildings. European Committee for Standardization, Brussels.

47. fib, 2010, Model Code for Concrete Structures. Fédération Internationale du Béton / International Federation for Structural Concrete, Lausanne.

48. Italian Ministry of Infrastructure and Transportation, 2018, Aggiornamento Norme Tecniche per le Costruzioni (DLGS 17/01/2018 – NTC 2018), Rome.

49. Mathcad 14 User’s guide, (2007), Mathsoft Inc., Cambridge, Massachusetts.