Title: Calcined Clay-Based Mineral Addition for the Production of Structural Concrete

Author(s): J. Fernando Martirena, Eilys Valdes, Adrian Alujas, and Karen Scrivener

Publication: Symposium Paper

Volume: 330

Issue:

Appears on pages(s): 189-196

Keywords: calcined clay; cement; pozzolan; grinding; hydration; concrete.

DOI: 10.14359/51711250

Date: 9/26/2018

Abstract:

This paper presents the results of the work to develop a mineral addition produced with a blend of 60% of calcined clay of kaolinitic origin, 30% of limestone and 10% of gypsum, to be added as Supplementary Cementitious Material directly while mixing concrete. The clay used has a kaolinite content within 40-50%, and has been activated at 800°C. The three components have been interground at a ball mill. The influence of the addition on cement hydration has been studied aided by Isothermal calorimetry of cement pastes having mineral additions of 35% and 50% per weight. Concrete with the minimum cement content required for the most aggressive exposure class (350 kg/m3) has been cast and mineral additions of 17% and 34% per weight have been made. Concrete strength went above 45 MPa, despite having the minimum cement content.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer