Abstract:
The production of sustainable building materials, such as concrete, has drawn increasing attention in the last decade. Breakthroughs in the development of new admixtures, optimized mix designs, innovative concrete management systems, together with a deeper understanding of the best-mode usage of admixtures with different cementitious materials have resulted in the production of sustainable concrete with better performance at a lower cost. This paper presents three approaches for producing sustainable concrete: (1) introduction of a new class of admixture systems that produce control flow concrete or concrete with flow characteristics of self-consolidating concrete (SCC) without using high cement content, (2) minimization of polycarboxylate ether/ester (PCE) and cement usage through better understanding of the interaction between PCEs and sulfates and (3) use of in-transit concrete management systems (iCMS) to consistently deliver concrete that will meet desired specifications with minimal over-design.
Related References:
1. Flatt, R. J.; Roussel, N.; and Cheeseman, C., “Concrete: An eco-material that needs to be improved,” Journal of the European Ceramic Society, V. 32, No. 11, 2012, pp. 2787-2798. doi: 10.1016/j.jeurceramsoc.2011.11.012
2. Aitcin, P.-C., and Flatt, R., “Science and Technology of Concrete Admixtures,” 1st Edition, Woodhead Publishing, 2016.
3. Cheung, J.; Jeknavorian, A.; Roberts, L.; and Silva, D., “Impact of admixtures on the hydration kinetics of Portland cement,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1289-1309. doi: 10.1016/j.cemconres.2011.03.005
4. Cheung, J.; Roberts, L.; and Liu, J., “Admixtures and Sustainability,” Cement and Concrete Research, In Press doi.org/10.1016/j.cemconres.2017.04.011.10.1016/j.cemconres.2017.04.011
5. Berodier, E.; Burns, E.; Cheung, J.; Gibson, L.; and Roberts, L., “Robust production of sustainable concrete through the use of admixtures and in-transit concrete management systems,” Cement and Concrete Composites, 2018, doi: , In press.10.1016/j.cemconcomp.2018.01.008
6. Yamada, K.; Ogawa, S.; and Hanehara, S., “Controlling of the Adsorption and Dispersing Force of Polycarboxylate-type Superplasticizer by Sulfate Ion Concentration in Aqueous Phase,” Cement and Concrete Research, V. 31, No. 3, 2001, pp. 375-383. doi: 10.1016/S0008-8846(00)00503-2
7. Roussel, N., ““A thixotropy model for fresh fluid concretes: Theory, validation and applications” Cement and Concrete Research, V. 36, No. 10, 2006, pp. 1797-1806 and Khayat, “Viscosity-enhancing admixtures for cement-based materials — An overview,” Cement and Concrete Composites, V. 20, No. 2-3, 1998, pp. 171-188.
8. Burns, E. G.; Rieder, K.-A.; Curto, J. W.; and Tregger, N., “The Rheology of Control Flow C,” Concrete International, V. 40, No. 1, 2018, p. 43
9. Ferraris, C. F.; Billberg, P.; Ferron, R.; Feys, D.; Hu, J.; Kawashima, S.; Koehler, E.; Sonebi, M.; Tanesi, J.; and Tregger, N., “Role of Rheology in Achieving Successful Concrete Performance,” Concrete International, V. 39, No. 6, June 2017, pp. 43-51.
10. Feys, D.; Wallevik, J.; Yahia, A.; Khayat, K.; and Wallevik, O., “Extension of the Reiner-Riwlin Equation to Determine Modified Bingham Parameters Measured in Coaxial Cylinders Rheometers,” Materials and Structures, V. 46, No. 1-2, 2013, pp. 289-311. doi: 10.1617/s11527-012-9902-6
11. Feys, D.; De Schutter, G.; Khaya, K. H.; and Verhoeven, R., “Changes in rheology of self-consolidating concrete induced by pumping,” Materials and Structures, V. 49, No. 11, 2016, pp. 4657-4677. doi: 10.1617/s11527-016-0815-7
12. Marchon, D.; Sulser, U.; Eberhardt, A.; and Flatt, R. J., “Molecular Design of Comb-shaped Polycarboxylate Dispersants for Environmentally Friendly Concrete,” Soft Matter, V. 9, No. 45, 2013, pp. 10719-10728. doi: 10.1039/c3sm51030a
13. Marchon, D.; Mantellato, S.; Eberhardt, A. B.; and Flatt, R. J., Adsorption of Chemical Admixtures, in: Sci. Technol. Concr. Admixtures, Woodhead Publishing, 2016, pp. 219–256.
14. Plank, J.; Zhimin, D.; Keller, H.; Hössle, F.; and Seidl, W., “Fundamental Mechanisms for Polycarboxylate Intercalation into C3A Hydrate Phases and the Role of Sulfate Present in Cement,” Cement and Concrete Research, V. 40, No. 1, 2010, pp. 45-57. doi: 10.1016/j.cemconres.2009.08.013
15. Dalas, F.; Nonat, A.; Pourchet, S.; Mosquet, M.; Rinaldi, D.; and Sabio, S., “Tailoring the Anionic Function and the Side Chains of Comb-like Superplasticizers to improve their Adsorption,” Cement and Concrete Research, V. 67, 2015, pp. 21-30. doi: 10.1016/j.cemconres.2014.07.024
16. Dalas, F.; Pourchet, S.; Rinaldi, D.; Nonat, A.; Sabio, S.; and Mosquet, M., “Modification of the Rate of Rormation and Surface Area of Ettringite by Polycarboxylate Ether Superplasticizers during Early C3A-CaSO4 Hydration,” Cement and Concrete Research, V. 69, 2015, pp. 105-113. doi: 10.1016/j.cemconres.2014.12.007
17. Suraneni, P., and Flatt, R. J., “Use of Micro-reactors to obtain New Insights into the Factors Influencing Tricalcium Silicate Dissolution,” Cement and Concrete Research, V. 78, 2015, pp. 208-215. doi: 10.1016/j.cemconres.2015.07.011
18. Marchon, D., “Controlling Cement Hydration Through The Molecular Structure Of Comb Copolymer Superplasticizers”, ETHZ, Zurich, 2016.
19. Marchon, D.; Juilland, P.; Gallucci, E.; Frunz, L.; and Flatt, R. J., “Molecular and Submolecular Scale Effects of Comb-copolymers on Tri-calcium Silicate Reactivity: Toward Molecular design,” Journal of the American Ceramic Society, V. 100, No. 3, 2017, pp. 817-841. doi: 10.1111/jace.14695
20. Giraudeau, C.; d’Espinose de Lacaillerie, J. B.; Zied, S.; Andre, N.; and Robert, F., “Surface and Intercalation Chemistry of Polycarboxylate Copolymers in Cementitious Systems,” Journal of the American Ceramic Society, V. 92, No. 11, 2009, pp. 2471-2488. doi: 10.1111/j.1551-2916.2009.03413.x
21. Tregger, N., “Automated slump management technology for consistent quality concrete, in: Transit Qual. Control”, ACI 238 Work. Fresh Concr. - ACI Conv. Spring, 2015.
22. Koehler, E. P., and Roberts, M. F., “Effects of in-transit addition of superplasticizer,” Proceedings of the 10th International Conference on Superplasticizers and Other Chemical Admixtures in Concrete, Prague, Czech, October, 2012.
23. Koehler, E., Sostaric, J. and Durning, T., “In-transit process control for ready mixed concrete,” Concrete inFocus, V. 9, No. 4, July/August, 2010, pp. 18-19.
24. Katzeff, D., “SensoCrete system for ready mixed concrete trucks,” Concrete International, V. 34, No. 12, December 2012, pp. 52-54.
25. Beaupre, D., “Mixer-mounted probe measures concrete workability,” Concrete International, V. 34, No. 9, September 2012, pp. 2-5.
26. Hammond, G. P., and Jones, C., “Embodied energy and carbon in construction materials,” Institution of Civil Engineers, V. 161, No. 2, 2008, pp. 87-98. doi: 10.1680/ener.2008.161.2.87