Durability of Structures Made of or Strengthened using Textile Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability of Structures Made of or Strengthened using Textile Reinforced Concrete

Author(s): Viktor Mechtcherine

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 54.1-54.10

Keywords: corrosion resistance, durability concept, multiple cracking, transport properties, textile reinforced concrete

DOI: 10.14359/51711037

Date: 8/10/2018

Abstract:
Textile-reinforced concrete (TRC) has great potential for application in structures exposed to severe mechanical or environmental loading. This article presents an overview of the current knowledge available on the durability of this composite and its components. An additional focus is centered on the protection of steel reinforcement, such as in the case of the strengthening or repair of RC structures using TRC. In doing this, the transport properties of TRC in the cracked state, its long-term tensile strength and strain capacity, and resistance to aggressive environments have been identified as critical parameters. Current knowledge indicates that TRC can exhibit over the long term high mechanical performance and favorable transport properties when cracked. While the superior resistance of TRC to aggressive environments is to be expected when compared to ordinary concrete, there is little information available on the effects of aggressive environments on the mechanical properties of the material. Since TRC is still a relatively new material, there is no information available on its long-term performance in the field. To be able to utilize the superior qualities of TRC fully, it will be necessary to develop a realistic and reliable performance-based durability design concept for structures made of or strengthened by TRC. This paper is an attempt to provide elements for such a framework.

Related References:

1. Brameshuber, W. editor (2006), Textile Reinforced Concrete: report no. 036 of the RILEM State-of-the-Art Report, RILEM Technical Commitee 201-TRC.

2. Butler, M., Lieboldt, M. and Mechtcherine, V. (2010a) ‘Application of Textile-Reinforced Concrete (TRC) for Structural Strengthening and in Prefabrication’, in Advances in Cement-based Materials, Taylor & Francis Group, London, 127-136.

3. Inaguma, H., Seki, M., Suda, K. and Rokugo, K. (2006), ‘Experimental study on crack-bridging ability of ECC for repair under train loading’, in Proceedings PRO 49 of International RILEM Workshop on HPFRCC in Structural Applications, Honolulu, US. RILEM Publications S.A.R.L.; 499-508.

4. European Brite-Euram Programm (2000), Probabilistic Performance Based Durability Design of Concrete Structures. Report no. BE95-1347/R17 of the DuraCrete Final Technical Report.

5. fib bulletin 34 (2006), Model code for Service Life Design, International Federation for Structural Concrete (fib); Lausanne.

6. Altmann, F. and Mechtcherine, V. (2013) ‘Durability design strategies for new cementitious materials’, in Cement and Concrete Research, 54, 114-125.

7. Altmann, F., Sickert, J.-U., Mechtcherine, V. and Kaliske, M. (2012) ‘A fuzzy-probabilistic durability concept for strain-hardening cement-based composites (SHCCs) exposed to chlorides: Part 1: Concept development’, in Cement and Concrete Composites, 34, 754-762.

8. Li, V.C. and Stang, H. (2004) ‘Elevating FRC material ductility to infrastructure durability’, in Proceedings PRO 39 of BEFIB; Varenna, Italy. RILEM Publications S.A.R.L.; 171-186.

9. Mechtcherine, V. and Lieboldt, M. (2011) ‘Permeation of water and gases through cracked textile reinforced concrete’, in Cement & Concrete Composites, 33, 725-734.

10. Barhum, R. and Mechtcherine, V. (2013) ‘Influence of short dispersed and short integral glass fibres on the mechanical behaviour of textile-reinforced concrete’, in Materials and Structures, 46, 557-572.

11. Scheffler, C., Gao, S.L., Plonka, R., Mäder, E., Hempel, S., Butler, M. and Mechtcherine, V. (2009), ‘Interphase modification of alkali-resistant glass fibres and carbon fibres for textile reinforced concrete I: Fibre properties and durability’, in Composite Science and Technology, 69, 531-538.

12. Butler, M., Mechtcherine, V. and Hempel, S. (2009b) ‘Experimental investigations on the durability of fibre- matrix interfaces in textile-reinforced concrete’, in Cement and Concrete Composites, 31(4), 221-231.

13. Butler, M., Mechtcherine, V. and Hempel, S. (2010b), ‘Durability of textile-reinforced concrete made with AR glass fibre - Effect of the matrix composition’, in Materials and Structures, 43, 1351-1368.

14. Butler, M., Hempel, S. and Mechtcherine, V. (2009a), ‘Zeitliche Entwicklung des Verbundes von AR-Glas- und Kohlenstofffaser-Multifilamentgarnen in zementgebundenen Matrices‘, in Curbach M and Jesse F (eds), Proc. 4th Colloquium on Textile Reinforced Structures (CTRS4), Dresden, 213-226.

15. Hempel, S., Butler, M. and Mechtcherine, V. (2015), ‘Bond behaviour and durability of basalt fibres in cementitious matrices’, RILEM Proc. PRO 98, W. Brameshuber (ed.), RILEM Publications S.A.R.L., 225-234.

16. Wagner, C., Villmann, B., Slowik, V., Mechtcherine, V. (2017) ‘Water permeability of cracked strain-hardening cement-based composites’, Cement and Concrete Composites 82 (2017) 234-241.

17. Lieboldt, M. and Mechtcherine, V. (2013) ‘Capillary transport of water through textile-reinforced concrete applied in repairing and/or strengthening cracked RC structures’, in Cement and Concrete Research, 52, 53-62. 18. Lieboldt, M. (2012) Transport of liquids and gases in Textile Reinforced Concrete, Doctoral thesis, Technische Universität Dresden, Schriftenreihe des Instituts für Baustoffe, Heft 2012/1 (in German).

19. Lawrence, C.D. (1986) ‘Measurements of permeability’, in Proceedings of 8th International Congress on the Chemistry of Cement, Rio de Janeiro, Brazil. FINEP; Vol. V., 29-34.

20. Freitag, S., Beer, M., Jesse, F. and Weiland, S. (2006) ‘Experimental investigation and prediction of long-term behavior of Textile Reinforced Concrete for strengthening’, in Hegger J, Brameshuber W and Will N. (eds), Textile Reinforced Concrete – Proceedings of the 1st International RILEM Conference, Aachen, RILEM, 121-130.