Title: Who is Watching Out for the Cylinders?

Author(s): Karthik H. Obla, Orville R. (Bud) Werner, John L. Hausfeld, Kevin A. MacDonald, Gregory D. Moody, and Nicholas J. Carino

Publication: Concrete International

Volume: 40

Issue: 8

Appears on pages(s): 28-35

Keywords: curing, strength testing, test cylinders, specifications

DOI:

Date: 8/1/2018

Abstract:
Standard curing involves initial curing at the job site under stipulated conditions. Field observations, however, show that on-site initial curing is often not done in accordance with ASTM C31/C31M. It should be possible to improve initial curing of acceptance test specimens by implementing the recommendations in this article.