International Concrete Abstracts Portal

  


Title: Confinement of Concrete Columns with SRG

Author(s): Christian Carloni, Mattia Santandrea, Imohamed Ali Omar Imohamed, Lesley H. Sneed

Publication: Symposium Paper

Volume: 324

Issue:

Appears on pages(s): 8.1-8.12

Keywords: Composites, Concrete, Steel reinforced grout, Confinement.

DOI: 10.14359/51702360

Date: 4/1/2018

Abstract:
In this study, the behavior of concrete compressive members confined by steel reinforced grout (SRG) is investigated. An experimental study was carried out to understand the behavior of short concrete prisms with a square cross-section confined by SRG subjected to a monotonic concentric compressive load. Test parameters considered in this study are the density of steel fibers, number of layers, corner condition, number of overlapping faces, and length of the reinforcement. The effectiveness of the confinement is evaluated in terms of peak stress with respect to unconfined prisms. SRG confinement is shown to improve the compressive strength of concrete prisms relative to the unconfined condition. An increase in the number of confinement layers results in an increase in the compressive strength and energy absorption.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer