Title: Development of Roller Compacted Concrete Mixtures for Bureau of Reclamation Mass Concrete Construction

Author(s): Timothy P. Dolen and kurt F. Von Fay

Publication: Symposium Paper

Volume: 141

Issue:

Appears on pages(s): 133-164

Keywords: air entrainment; bleeding (concrete); bonding; cohesion; compressive strength; construction; cores; creep properties; research; density (mass/volume); durability; mass concrete; mix proportioning; permeability; roller compacted concrete; shear properties;

DOI: 10.14359/3993

Date: 12/1/1993

Abstract:
The Bureau of Reclamation has proportioned roller compacted concrete (RCC) mixtures since 1979, beginning with the Upper Stillwater Dam Project. Reclamation's research and project-related RCC investigations cover a variety of structures and varying site conditions. Reclamation proportions RCC mixtures to meet both fresh and hardened concrete properties. This assures construction of high-quality concrete structures. Ongoing research has continued to identify specific properties of RCC, such as bond strength, freeze-thaw durability, and thermal properties that significantly affect the performance of these structures. Paper summarizes RCC mixture proportions and properties of fresh and hardened concrete from Reclamation's RCC research and project activities.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer