Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Thermal Conductivity and Thermal Expansion Coefficients of Concrete as a Function of Temperature and Humidty
Author(s): J.C. Marechal
Publication: Symposium Paper
Volume: 34
Issue:
Appears on pages(s): 1047-1058
Keywords: aggregates; concretes; desorption; diffusion; high temperature; humidity; low temperature; moisture content; nuclear reactor containment; research; temperature; thermal conductivity; thermal expansion
DOI: 10.14359/18105
Date: 1/1/1972
Abstract: Thermal conductivity and thermal expansion coefficients were measured on various concretes according to temperature and the loss of water up to 500 C. The results are set out and discussed in relation to the other properties previously mentioned.