Title:
Controlling Concrete During Hot and Cold Weather
Author(s):
John M. Scanlon
Publication:
Symposium Paper
Volume:
104
Issue:
Appears on pages(s):
241-260
Keywords:
cold weather construction; concretes; curing; hot weather construction; insulation; mix proportioning; quality assurance; quality control; General
DOI:
10.14359/1732
Date:
10/1/1987
Abstract: