Title:
Behavior of Ferrocement Reinforcement in Tension
Author(s):
Antonio Nanni and Ronald F. Zollo
Publication:
Materials Journal
Volume:
84
Issue:
4
Appears on pages(s):
273-277
Keywords:
ferrocement; modulus of elasticity; reinforcing steels; strains; strength; tension tests; welded wire fabric; yield point; Materials Research
DOI:
10.14359/1615
Date:
7/1/1987
Abstract:
Ferrocement makes use of layers of reinforcement that are most often in the form of welded or woven wire mesh and expanded metal. These materials, in the sizes and gages commonly used, are not generally intended for applications in engineered systems and,