Title:
ACI-ASCC Survey on Portland-Limestone Cement Concrete
Author(s):
James Klinger, Kevin A. MacDonald, Jerry A. Holland, Scott M. Tarr, Beverly A. Garnant, and Bruce A. Suprenant
Publication:
Concrete International
Volume:
46
Issue:
2
Appears on pages(s):
27-36
Keywords:
question, problem, floor, slab
DOI:
Date:
2/1/2024
Abstract:
A Joint ACI-ASCC Task Group developed a survey to gather information regarding the construction of concrete floors and slabs using ordinary portland cement (OPC) and portland-limestone cement. This article presents 15 survey questions and a summary of responses provided by 173 respondents, as well as information from previously conducted surveys.