Title: Proposed Data Sheet for Alternative Cementitious Materials

Author(s): Terence C. Holland and Kenneth C. Hover

Publication: Concrete International

Volume: 42

Issue: 8

Appears on pages(s): 43-47

Keywords: cement, code, requirements, supplier

Date: 8/1/2020

Abstract:
Based on research data, new materials are being proposed for use as alternative cements or alternative supplementary cementitious materials. However, bringing new materials to market is difficult, time-consuming, and expensive. The product data sheet proposed in this article will guide potential suppliers through the testing and documentation that will be required to market alternative cementitious materials.




  

Please enter this 5 digit unlock code on the web page.