Title:
Potential for Using Waste Recycled Glass in Engineered Cementitious Composites
Author(s):
Hocine Siad , Mohamed Lachemi, Mustafa Sahmaran, K. M Anwar Hossain
Publication:
Symposium Paper
Volume:
320
Issue:
Appears on pages(s):
34.1-34.14
Keywords:
Glass Powder; Glass Sand; Self-healing; Engineered Cementitious Composites
DOI:
10.14359/51701072
Date:
8/1/2017
Abstract:
This paper outlines a detailed study on the use of Waste Glass Powder (WGP) and Waste Glass Sand (WGS) with Fly Ash (FA) and Silica Sand (SS) replacements in Engineered Cementitious Composites (ECC). It investigates the effect of different replacement levels of WGP and WGS on the mechanical, physical and selfhealing efficiency of ECC’s. For this purpose, mixtures were prepared with 0, 15, 30, 45 and 60% of FA
replacement by weight of WGP, and SS was replaced with 0, 25, 50, 75 and 100% by weight of WGS. Compressive and flexural strengths, mid-span beam deflection capacity, rapid chloride penetrability and resistivity were tested to assess the mechanical, physical and self-healing performances of different sound and preloaded specimens. The results of this study showed the possibility of replacing FA by WGP, and SS by WGS in the production of different ECC’s. Optimum mechanical, physical and self-healing characteristics were obtained for
ECC mixtures including up to 30% of WGP or up to 50% of WGS replacement level. Alkalis and aluminum based-C-S-H with low Ca/Si was the main healing product in the healed crack lines of WGP- and WGS- based ECC’s.
Related References:
1. Li, V. C., “On Engineered Cementitious Composites (ECC) a review of the material and its applications,”Journal of advanced concrete technology, Vol 1, No. 3, 2003, pp: 215-230.
2. Sahmaran, M., Yildirim, G., and Erdem, T.K., “Self-healing capability of cementitious compositesincorporating different supplementary cementitious materials,” Cement and concrete composites, Vol 35, No. 1.2013, pp:89-101.
3. Ozbay, E., Sahmaran, M., Lachemi, M., and Yucel, H.E., “Self-Healing of microcracks in high-volume flyash-incorporated engineered cementitious composites,” ACI Materials Journal, Vol 110, No.1. 2013, pp.33-43.
4. Zhu, Y., Yang, Y., and Yao, Y., “Use of slag to improve mechanical properties of engineered cementitiouscomposites (ECCs) with high volumes of fly ash,” Construction and Building Materials, Vol 36. 2012, pp. 1076-1081.
5. Huang, X., Ranade, R., Ni, W., and Li, V. C., “Development of green engineered cementitious compositesusing iron ore tailings as aggregates,” Construction and Building Materials, Vol 44. 2013, pp. 757-764.
6. Sahmaran, M., Lachemi, M., Hossain, K., Ranade, R. and Li, V.C., “Influence of aggregate type and size onductility and mechanical properties of engineered cementitious composites,” ACI Materials Journal, Vol 106, No.3. 2009, pp. 308-316.
7. Lepech, M.D., Keoleian, G.A., Qian, S. and Li, V.C., 2008, “Design of green engineered cementitiouscomposites for pavement overlay applications,” In Proceedings of the First International Symposium on LifeCycle Civil Engineering, pp. 10-14.
8. Siad, H., Alyousif, A., Keskin, O.K., Keskin, S.B., Lachemi, M., Sahmaran, M. and Hossain, K.M.A.,“Influence of limestone powder on mechanical, physical and self-healing behavior of Engineered CementitiousComposites,” Construction and Building Materials, Vol 99. 2015, pp.1-10.
9. Al-Najjar, Y., Yesilmen, S., Al-Dahawi, A.M., Sahmaran, M., Yildirim, G., Lachemi, M., and Amleh, L.,“Physical and Chemical Actions of Nano-Mineral Additives on Properties of High-Volume Fly Ash EngineeredCementitious Composites,” ACI Materials Journal, Vol 113, No 6. 2016, pp. 791-801
10. Tagnit-Hamou, A., and Bengougam, A., “Glass powder as a supplementary cementitious material,” Concreteinternational, Vol 34, No 3. pp. 56-61.
11. Tagnit-Hamou, A., Soliman, N., Omran, A.F., Mousa, M.T., Gauvreau, N., and Provencher, M., “Novel ultrahigh-performance glass concrete,” Concrete International, Vol 37, No. 3, 2015, pp. 41-47.
12. Bazant, Z.P., Zi, G., and Meyer, C., “Fracture mechanics of ASR in concretes with waste glass particles ofdifferent sizes,” Journal of Engineering Mechanics. Vol 126. 2000, pp. 226-232.
13. Shao, Y., Lefort, T., Moras, S., and Damian, R., “Studies on concrete containing ground waste glass,” CemConcr Res, Vol 30, No. 1, pp. 91–100.
14. Liu, S., Wang, S., Tang, W., Hu, N. and Wei, J., (2015) “Inhibitory Effect of Waste Glass Powder on ASRExpansion Induced by Waste Glass Aggregate,” Materials. Vol 8. 2000, pp. 6849-6862.
15. ASTM (American Society for Testing and Materials). Standard specification for Portland cement. ASTMC150 2012 West Conshohocken, PA.
16. ASTM (American Society for Testing and Materials). Standard Specification for Coal Fly Ash and Raw orCalcined Natural Pozzolan for Use in Concrete. ASTM C618 2012A, West Conshohocken, PA.
17. ASTM (American Society for Testing and Materials). Standard Test Method for Potential Alkali Reactivityof Aggregates (Mortar-Bar Method). ASTM C1260 - 14, 2014, West Conshohocken, PA.
18. Özbay, E., Sahmaran, M., Yücel, H.E., Erdem, T.K., Lachemi, M. and Li, V.C., “Effect of sustained flexuralloading on self-healing of engineered cementitious composites. Journal of Advanced Concrete Technology, Vol11, No. 5. 2013, pp.167-179.
19. ASTM (American Society for Testing and Materials). Standard Test Method for Electrical Indication ofConcrete’s Ability to Resist Chloride Ion Penetration, ASTM C1202, 2012, West Conshohocken, PA.
20. Vaitkevicius, V., Šerelis, E. and Hilbig, H., “The effect of glass powder on the microstructure of ultra highperformance concrete,” Construction and Building Materials, Vol 68. 2014. pp.102-109.
21. Siad, H., Lachemi, M., Sahmaran, M. and Hossain, K.M.A., “Effect of glass powder on sulfuric acidresistance of cementitious materials,” Construction and Building Materials, Vol 113. 2016, pp.163-173.
22. Sahmaran, M., Yucel, H. E., Demirhan, S., Arik, M. T., and Li, V. C., “Combined Effect of Aggregate andMineral Admixtures on Tensile Ductility of Engineered Cementitious Composites.” ACI Mat. J., Vol 109, No. 6. 2012, pp.627-638.
23. Sahmaran, M., Lachemi, M., Hossain, K., Ranade, R. and Li, V.C., “Influence of aggregate type and size onductility and mechanical properties of engineered cementitious composites. ACI Materials Journal, Vol 106, No. 3. 2009,pp.308-316.
24. Jain, J.A. and Neithalath, N., “Chloride transport in fly ash and glass powder modified concretes–influenceof test methods on microstructure. Cement and Concrete Composites, Vol 32, No. 2. 2010, pp.148-156.
25. Hansson, I.L.H. and Hansson, C.M., “Electrical resistivity measurements of Portland cement basedmaterials. Cement and Concrete Research,” Vol 13, No. 5. 1983, pp.675-683.
26. Fan, S., and Li, M. “X-ray computed microtomography of three-dimensional microcracks and self-healingin engineered cementitious composites,” Smart Mater Struct, Vol 24, No. 1. 2015, pp. 1-14.